A novel and efficient method for the extraction of cellulose fibers from Spanish broom(Spartium junceum L.) is presented. The method is based on the sequential combination between an initial chemical stage (alkaline digestion) and a subsequent physical–chemical stage, consisting of compression with hot air in an autoclave followed by rapid decompression (DiCoDe process, digestion–compression–decompression). The alkaline mother liquor deriving from the initial digestion step can be conveniently recycled after centrifugation followed by ultrafiltration. The process is characterized by the production of fibers with excellent physical–chemical properties, such as high mechanical resistance and high elasticity, and rapid production times. The fibers obtained after the DiCoDe process can be further softened and whitened by means of enzymatic digestion. Fibers were morphologically characterized by scanning electron microscopy (SEM), while their composition and physical–chemical properties were determined by conventional methods, including colorimetry, TAPPI protocols, IR spectroscopy, and X-ray diffractometry.

A new physical-chemical process for the efficient production of cellulose fibers from Spanish broom (Spartium junceum L.)

GABRIELE, Bartolo;CHIDICHIMO, Giuseppe;
2010-01-01

Abstract

A novel and efficient method for the extraction of cellulose fibers from Spanish broom(Spartium junceum L.) is presented. The method is based on the sequential combination between an initial chemical stage (alkaline digestion) and a subsequent physical–chemical stage, consisting of compression with hot air in an autoclave followed by rapid decompression (DiCoDe process, digestion–compression–decompression). The alkaline mother liquor deriving from the initial digestion step can be conveniently recycled after centrifugation followed by ultrafiltration. The process is characterized by the production of fibers with excellent physical–chemical properties, such as high mechanical resistance and high elasticity, and rapid production times. The fibers obtained after the DiCoDe process can be further softened and whitened by means of enzymatic digestion. Fibers were morphologically characterized by scanning electron microscopy (SEM), while their composition and physical–chemical properties were determined by conventional methods, including colorimetry, TAPPI protocols, IR spectroscopy, and X-ray diffractometry.
2010
Biomaterials; Fibers extraction; Spanish broom; Cellulose
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.11770/142995
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 47
  • ???jsp.display-item.citation.isi??? 44
social impact